hrcak mascot   Srce   HID

Original scientific paper
https://doi.org/10.15644/asc47/2/2

Fluoride Release from Hard Dental Tissue Restorative Materials

Danijela Vrček ; Private dental practice, Varaždin, Croatia
Goranka Prpić-Mehičić ; Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Zagreb, Croatia
Željko Verzak ; Department of Pediatric Dentistry, School of Dental Medicine, University of Zagreb, Zagreb, Croatia
Jurica Vrček ; Private dental practice, Varaždin, Croatia
Jurica Matijević ; Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Zagreb, Croatia
Kata Rošin-Grget ; Department of Pharmacology, School of Dental Medicine, University of Zagreb, Zagreb, Croatia

Fulltext: english, pdf (370 KB) pages 111-119 downloads: 343* cite
APA 6th Edition
Vrček, D., Prpić-Mehičić, G., Verzak, Ž., Vrček, J., Matijević, J. & Rošin-Grget, K. (2013). Fluoride Release from Hard Dental Tissue Restorative Materials. Acta stomatologica Croatica, 47 (2), 111-119. https://doi.org/10.15644/asc47/2/2
MLA 8th Edition
Vrček, Danijela, et al. "Fluoride Release from Hard Dental Tissue Restorative Materials." Acta stomatologica Croatica, vol. 47, no. 2, 2013, pp. 111-119. https://doi.org/10.15644/asc47/2/2. Accessed 3 Aug. 2021.
Chicago 17th Edition
Vrček, Danijela, Goranka Prpić-Mehičić, Željko Verzak, Jurica Vrček, Jurica Matijević and Kata Rošin-Grget. "Fluoride Release from Hard Dental Tissue Restorative Materials." Acta stomatologica Croatica 47, no. 2 (2013): 111-119. https://doi.org/10.15644/asc47/2/2
Harvard
Vrček, D., et al. (2013). 'Fluoride Release from Hard Dental Tissue Restorative Materials', Acta stomatologica Croatica, 47(2), pp. 111-119. https://doi.org/10.15644/asc47/2/2
Vancouver
Vrček D, Prpić-Mehičić G, Verzak Ž, Vrček J, Matijević J, Rošin-Grget K. Fluoride Release from Hard Dental Tissue Restorative Materials. Acta stomatologica Croatica [Internet]. 2013 [cited 2021 August 03];47(2):111-119. https://doi.org/10.15644/asc47/2/2
IEEE
D. Vrček, G. Prpić-Mehičić, Ž. Verzak, J. Vrček, J. Matijević and K. Rošin-Grget, "Fluoride Release from Hard Dental Tissue Restorative Materials", Acta stomatologica Croatica, vol.47, no. 2, pp. 111-119, 2013. [Online]. https://doi.org/10.15644/asc47/2/2
Fulltext: croatian, pdf (370 KB) pages 111-119 downloads: 405* cite
APA 6th Edition
Vrček, D., Prpić-Mehičić, G., Verzak, Ž., Vrček, J., Matijević, J. & Rošin-Grget, K. (2013). Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva. Acta stomatologica Croatica, 47 (2), 111-119. https://doi.org/10.15644/asc47/2/2
MLA 8th Edition
Vrček, Danijela, et al. "Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva." Acta stomatologica Croatica, vol. 47, no. 2, 2013, pp. 111-119. https://doi.org/10.15644/asc47/2/2. Accessed 3 Aug. 2021.
Chicago 17th Edition
Vrček, Danijela, Goranka Prpić-Mehičić, Željko Verzak, Jurica Vrček, Jurica Matijević and Kata Rošin-Grget. "Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva." Acta stomatologica Croatica 47, no. 2 (2013): 111-119. https://doi.org/10.15644/asc47/2/2
Harvard
Vrček, D., et al. (2013). 'Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva', Acta stomatologica Croatica, 47(2), pp. 111-119. https://doi.org/10.15644/asc47/2/2
Vancouver
Vrček D, Prpić-Mehičić G, Verzak Ž, Vrček J, Matijević J, Rošin-Grget K. Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva. Acta stomatologica Croatica [Internet]. 2013 [cited 2021 August 03];47(2):111-119. https://doi.org/10.15644/asc47/2/2
IEEE
D. Vrček, G. Prpić-Mehičić, Ž. Verzak, J. Vrček, J. Matijević and K. Rošin-Grget, "Otpuštanje fluorida iz materijala za nadoknadu tvrdih zubnih tkiva", Acta stomatologica Croatica, vol.47, no. 2, pp. 111-119, 2013. [Online]. https://doi.org/10.15644/asc47/2/2

Abstracts
Aim: The aim of this in vitro study was to determine and to compare the level and dynamics of fluoride release in three types of current filling materials. Materials and methods: luoride release was measured in GC Kalore composite, glass ionomer GC Equia cement and Shofu Beautiful II giomer. 20 discs were made from each material (8 mm diameter, 2 mm thickness). Measurements were made during 10 weeks by an ion-selective electrode (ORION EA 940). The linear regression method was used in statistical data processing. Results: The GC Kalore composite released 1.29 ppm F- in 10 weeks of testing. Fluoride release decreased and after 4 weeks of testing, it became impossible to measure by ion-selective electrode. Glass ionomer cement, GC Equia released the greatest number of fluoride ions (24.512 ppm F-) and the greatest number of fluorides was released during the first 24 hours (6.8507 mgF- /L). Giomer Shofu Beautiful II released 4.685 ppm F-. Conclusion: The examined giomer released more fluorides than the composite material and therefore, it can be recommended as a material of choice for esthetic fillings in which the caries preventive effect is also important.

Keywords
Composite Resins; Glass Ionomer Cement; Fluorides; giomer