hrcak mascot   Srce   HID

Preliminary communication

Corrosion of the WE43 and MSR-B magnesium alloys in CO2

R. Przeliorz ; The Silesian University of Technology, Katowice, Poland
J. Piątkowski ; The Silesian University of Technology, Katowice, Poland

Fulltext: english, pdf (331 KB) pages 429-432 downloads: 265* cite
APA 6th Edition
Przeliorz, R. & Piątkowski, J. (2016). Corrosion of the WE43 and MSR-B magnesium alloys in CO2. Metalurgija, 55 (3), 429-432. Retrieved from https://hrcak.srce.hr/153639
MLA 8th Edition
Przeliorz, R. and J. Piątkowski. "Corrosion of the WE43 and MSR-B magnesium alloys in CO2." Metalurgija, vol. 55, no. 3, 2016, pp. 429-432. https://hrcak.srce.hr/153639. Accessed 18 Jun. 2019.
Chicago 17th Edition
Przeliorz, R. and J. Piątkowski. "Corrosion of the WE43 and MSR-B magnesium alloys in CO2." Metalurgija 55, no. 3 (2016): 429-432. https://hrcak.srce.hr/153639
Harvard
Przeliorz, R., and Piątkowski, J. (2016). 'Corrosion of the WE43 and MSR-B magnesium alloys in CO2', Metalurgija, 55(3), pp. 429-432. Available at: https://hrcak.srce.hr/153639 (Accessed 18 June 2019)
Vancouver
Przeliorz R, Piątkowski J. Corrosion of the WE43 and MSR-B magnesium alloys in CO2. Metalurgija [Internet]. 2016 [cited 2019 June 18];55(3):429-432. Available from: https://hrcak.srce.hr/153639
IEEE
R. Przeliorz and J. Piątkowski, "Corrosion of the WE43 and MSR-B magnesium alloys in CO2", Metalurgija, vol.55, no. 3, pp. 429-432, 2016. [Online]. Available: https://hrcak.srce.hr/153639. [Accessed: 18 June 2019]

Abstracts
The kinetics of WE43 and MSR-B magnesium alloys oxidation was tested in CO2 atmosphere. The measurement of the oxidation speed was conducted with continuous thermo gravimetric method in the eutectic melting temperature (530 °C). This temperature has been defined with the differential scanning calorimetric (DSC) method. The corrosion products were analyzed with Scanning Electron Microscopy (SEM) and Energy Disspersive X-ray Spectroscopy (EDS) methods. On the WE43 alloy the double layer scale is being created, with good protective properties. Under the scale layer the internal oxidation of the alloy takes place. The oxide layer on MSR-B alloy is thin and irregular.

Keywords
corrosion; cast magnesium alloys; oxidation; structure; CO2 atmosphere