hrcak mascot   Srce   HID

Izvorni znanstveni članak

Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel

A. Di Schino ; Università di Perugia, Dipartimento di Ingegneria, Perugia, Italy
R. Rufini ; Università di Perugia, Dipartimento di Ingegneria, Perugia, Italy

Puni tekst: engleski, pdf (216 KB) str. 272-274 preuzimanja: 133* citiraj
APA 6th Edition
Schino, A.D. i Rufini, R. (2018). Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel. Metalurgija, 57 (4), 272-274. Preuzeto s https://hrcak.srce.hr/201737
MLA 8th Edition
Schino, A. Di i R. Rufini. "Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel." Metalurgija, vol. 57, br. 4, 2018, str. 272-274. https://hrcak.srce.hr/201737. Citirano 14.12.2019.
Chicago 17th Edition
Schino, A. Di i R. Rufini. "Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel." Metalurgija 57, br. 4 (2018): 272-274. https://hrcak.srce.hr/201737
Harvard
Schino, A.D., i Rufini, R. (2018). 'Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel', Metalurgija, 57(4), str. 272-274. Preuzeto s: https://hrcak.srce.hr/201737 (Datum pristupa: 14.12.2019.)
Vancouver
Schino AD, Rufini R. Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel. Metalurgija [Internet]. 2018 [pristupljeno 14.12.2019.];57(4):272-274. Dostupno na: https://hrcak.srce.hr/201737
IEEE
A.D. Schino i R. Rufini, "Thermo-mechanical process parameters effect on a 9 % Cr-2 % W steel", Metalurgija, vol.57, br. 4, str. 272-274, 2018. [Online]. Dostupno na: https://hrcak.srce.hr/201737. [Citirano: 14.12.2019.]

Sažetak
In this paper the effect of thermo-mechanical parameters on the mechanical behavior of a 9 % Cr-2 % W steel is investigated by hot rolling and heat treatment on pilot scale. Results show a strong effect of reheating temperature before rolling on the material hardness, due to an increase of hardenability following the austenite grain growth. A poor effect of the hot reduction and of the following tempering temperature is detected in the total investigated deformation range. A loss of impact energy is found coupled with the hardness increase. The tensile properties values are strongly depending upon the tempering temperature and an increase of tensile yield stress (Rp0,2) and ultimate stress (Rm) have been recorded in tensile test carried on at T = 550°C and T = 650°C.

Ključne riječi
steel; thermo-mechanical process; microstructure; mechanical properties; rolling temperature