hrcak mascot   Srce   HID

Izvorni znanstveni članak

Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0

Nives Rinčić
Asja Čelebić
Ivo Baučić
Jasmina Stipetić
Esad Prohić
Slobodan Miko

Puni tekst: hrvatski, pdf (77 KB) str. 5-11 preuzimanja: 471* citiraj
APA 6th Edition
Rinčić, N., Čelebić, A., Baučić, I., Stipetić, J., Prohić, E. i Miko, S. (2003). Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0. Acta stomatologica Croatica, 37 (1), 5-11. Preuzeto s https://hrcak.srce.hr/2572
MLA 8th Edition
Rinčić, Nives, et al. "Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0." Acta stomatologica Croatica, vol. 37, br. 1, 2003, str. 5-11. https://hrcak.srce.hr/2572. Citirano 08.03.2021.
Chicago 17th Edition
Rinčić, Nives, Asja Čelebić, Ivo Baučić, Jasmina Stipetić, Esad Prohić i Slobodan Miko. "Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0." Acta stomatologica Croatica 37, br. 1 (2003): 5-11. https://hrcak.srce.hr/2572
Harvard
Rinčić, N., et al. (2003). 'Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0', Acta stomatologica Croatica, 37(1), str. 5-11. Preuzeto s: https://hrcak.srce.hr/2572 (Datum pristupa: 08.03.2021.)
Vancouver
Rinčić N, Čelebić A, Baučić I, Stipetić J, Prohić E, Miko S. Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0. Acta stomatologica Croatica [Internet]. 2003 [pristupljeno 08.03.2021.];37(1):5-11. Dostupno na: https://hrcak.srce.hr/2572
IEEE
N. Rinčić, A. Čelebić, I. Baučić, J. Stipetić, E. Prohić i S. Miko, "Otpuštanje iona iz bazne Co-Cr-Mo slitine in vitro u fosfatni pufer pH 6,0", Acta stomatologica Croatica, vol.37, br. 1, str. 5-11, 2003. [Online]. Dostupno na: https://hrcak.srce.hr/2572. [Citirano: 08.03.2021.]
Puni tekst: engleski, pdf (61 KB) str. 13-16 preuzimanja: 964* citiraj
APA 6th Edition
Rinčić, N., Čelebić, A., Baučić, I., Stipetić, J., Prohić, E. i Miko, S. (2003). The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0. Acta stomatologica Croatica, 37 (1), 13-16. Preuzeto s https://hrcak.srce.hr/2572
MLA 8th Edition
Rinčić, Nives, et al. "The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0." Acta stomatologica Croatica, vol. 37, br. 1, 2003, str. 13-16. https://hrcak.srce.hr/2572. Citirano 08.03.2021.
Chicago 17th Edition
Rinčić, Nives, Asja Čelebić, Ivo Baučić, Jasmina Stipetić, Esad Prohić i Slobodan Miko. "The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0." Acta stomatologica Croatica 37, br. 1 (2003): 13-16. https://hrcak.srce.hr/2572
Harvard
Rinčić, N., et al. (2003). 'The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0', Acta stomatologica Croatica, 37(1), str. 13-16. Preuzeto s: https://hrcak.srce.hr/2572 (Datum pristupa: 08.03.2021.)
Vancouver
Rinčić N, Čelebić A, Baučić I, Stipetić J, Prohić E, Miko S. The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0. Acta stomatologica Croatica [Internet]. 2003 [pristupljeno 08.03.2021.];37(1):13-16. Dostupno na: https://hrcak.srce.hr/2572
IEEE
N. Rinčić, A. Čelebić, I. Baučić, J. Stipetić, E. Prohić i S. Miko, "The Release of Ions from the Base Co-Cr-Mo Casting Alloy in vitro into the Phosphate Buffer at pH 6.0", Acta stomatologica Croatica, vol.37, br. 1, str. 13-16, 2003. [Online]. Dostupno na: https://hrcak.srce.hr/2572. [Citirano: 08.03.2021.]

Sažetak
Svrha rada bila je ispitati ponašanje WIRONIT® slitine u fosfatnom puferu pH 6,0 (kako bi se simulirala ljudska slina) kroz dulje razdoblje, te ustanoviti vrstu i količinu iona koji se otpuštaju iz slitine. Također se je željelo ustanoviti kako na otpuštanje iona utječe vrijeme izloženosti slitine djelovanju fosfatnoga pufera pH 6,0. U tu svrhu ispitano je 60 neobrađenih tvorničkih uzoraka WIRONIT® slitine promjera 8 mm i visine 15,8 mm. Otpuštanje iona mjereno je u deset razdoblja: 1, 2, 3, 4, 5, 6, 7, 14, 21 i 30 dana. Raščlambom otopina u kojima su bili uzorci ispitivane slitine s pomoću atomskoga emisijskog spektrofotometra s induciranom združenom plazmom (ICP-AES) utvrđeno je da su se u mjesec dana otpustili ioni kobalta (Co), kroma (Cr), željeza (Fe), cinka (Zn) i nikla (Ni). Iz uzoraka bazne Co-Cr-Mo slitine najviše se otpustilo iona kobalta, a najmanje iona željeza. Rezultati su pokazali da na otpuštanje svih pronađenih iona statistički znatno utječe vrijeme ekspozicije slitine fosfatnom puferu pH 6,0 (p<0,01).

Ključne riječi
otpuštanje iona; Co-Cr-Mo slitina

Hrčak ID: 2572

URI
https://hrcak.srce.hr/2572

[engleski]

Posjeta: 1.788 *