hrcak mascot   Srce   HID

Stručni rad

Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier

Ivo Senjanović ; Faculty of Mechanical Engineering
Joško Parunov ; Faculty of Mechanical Engineering
Smiljko Rudan ; Faculty of Mechanical Engineering

Puni tekst: engleski, pdf (5 MB) str. 290-297 preuzimanja: 1.712* citiraj
APA 6th Edition
Senjanović, I., Parunov, J. i Rudan, S. (2009). Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier. Brodogradnja, 60 (3), 290-297. Preuzeto s https://hrcak.srce.hr/43578
MLA 8th Edition
Senjanović, Ivo, et al. "Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier." Brodogradnja, vol. 60, br. 3, 2009, str. 290-297. https://hrcak.srce.hr/43578. Citirano 19.10.2021.
Chicago 17th Edition
Senjanović, Ivo, Joško Parunov i Smiljko Rudan. "Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier." Brodogradnja 60, br. 3 (2009): 290-297. https://hrcak.srce.hr/43578
Harvard
Senjanović, I., Parunov, J., i Rudan, S. (2009). 'Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier', Brodogradnja, 60(3), str. 290-297. Preuzeto s: https://hrcak.srce.hr/43578 (Datum pristupa: 19.10.2021.)
Vancouver
Senjanović I, Parunov J, Rudan S. Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier. Brodogradnja [Internet]. 2009 [pristupljeno 19.10.2021.];60(3):290-297. Dostupno na: https://hrcak.srce.hr/43578
IEEE
I. Senjanović, J. Parunov i S. Rudan, "Remedy for Misalignment of Bilobe Tank Heads in Liquefied Petroleum Gas Carrier", Brodogradnja, vol.60, br. 3, str. 290-297, 2009. [Online]. Dostupno na: https://hrcak.srce.hr/43578. [Citirano: 19.10.2021.]

Sažetak
The article describes the remedy for a misalignment of Y-joint in hemispherical and torispherical heads of the bilobe cargo tank on a Liquefi ed Petroleum Gas Carrier. The misalignment is the result of connecting relatively thin shells and production diffi culties. The measured rather large shell eccentricity in the Y-joint causes bending moment, which cannot be withstood by shells designed as membrane, and therefore it has to be controlled. The remedy of misalignment is
achieved by reinforcement of the Y-joint with inside and outside bars and knees. In this way stress concentration determined by the FEM analysis is reduced within the allowable stress given for secondary stress level.

Ključne riječi
LPG carrier; bilobe tank; misalignment; reinforcement; strength analysis; FEM