hrcak mascot   Srce   HID

Prethodno priopćenje

Oštećenje na čeličnoj tračničkoj osovini u eksploataciji

Oleh Yasniy   ORCID icon orcid.org/0000-0002-9820-9093 ; Ternopil Ivan Pul'uj State Technical University, Ruska Str. 56, 46001 Ternopil, Ukraine
Tomaž Vuherer ; University of Maribor, Faculty of Mechanical Engineering, Slovenia
Yuriy Pyndus ; Ternopil Ivan Pul'uj State Technical University, Ruska Str. 56, 46001 Ternopil, Ukraine
Andriy Sorochak ; Ternopil Ivan Pul'uj State Technical University, Ruska Str. 56, 46001 Ternopil, Ukraine
Ivan Samardžić ; Mechanical Engineering Faculty in Slavonski Brod, J. J. Strossmayer University of Osijek, Trg Ivane Brlić-Mažuranić 2, 35000 Slavonski Brod, Croatia

Puni tekst: engleski, pdf (554 KB) str. 87-90 preuzimanja: 473* citiraj
APA 6th Edition
Yasniy, O., Vuherer, T., Pyndus, Y., Sorochak, A. i Samardžić, I. (2011). In-service damage of railway steel axles. Tehnički vjesnik, 18 (1), 87-90. Preuzeto s https://hrcak.srce.hr/65930
MLA 8th Edition
Yasniy, Oleh, et al. "In-service damage of railway steel axles." Tehnički vjesnik, vol. 18, br. 1, 2011, str. 87-90. https://hrcak.srce.hr/65930. Citirano 25.02.2020.
Chicago 17th Edition
Yasniy, Oleh, Tomaž Vuherer, Yuriy Pyndus, Andriy Sorochak i Ivan Samardžić. "In-service damage of railway steel axles." Tehnički vjesnik 18, br. 1 (2011): 87-90. https://hrcak.srce.hr/65930
Harvard
Yasniy, O., et al. (2011). 'In-service damage of railway steel axles', Tehnički vjesnik, 18(1), str. 87-90. Preuzeto s: https://hrcak.srce.hr/65930 (Datum pristupa: 25.02.2020.)
Vancouver
Yasniy O, Vuherer T, Pyndus Y, Sorochak A, Samardžić I. In-service damage of railway steel axles. Tehnički vjesnik [Internet]. 2011 [pristupljeno 25.02.2020.];18(1):87-90. Dostupno na: https://hrcak.srce.hr/65930
IEEE
O. Yasniy, T. Vuherer, Y. Pyndus, A. Sorochak i I. Samardžić, "In-service damage of railway steel axles", Tehnički vjesnik, vol.18, br. 1, str. 87-90, 2011. [Online]. Dostupno na: https://hrcak.srce.hr/65930. [Citirano: 25.02.2020.]

Sažetak
U radu je istražen utjecaj temperature i mjesta zajeda uzorka na udarnu žilavost materijala tračničke osovine u eksploataciji. Dobiveni rezultati pokazuju obrnutu proporcionalnost ovisnosti udarne žilavosti o polumjeru zajeda na uzorcima. Smanjenjem temperature ispitivanja od +20 to –40 °C značajno se smanjuje udarna žilavost i udio žilavog loma.

Ključne riječi
oštećenje u eksploataciji; tračnička osovina; udarna žilavost; zajeda