Skoči na glavni sadržaj

Izvorni znanstveni članak

https://doi.org/10.15644/asc54/4/4

Fluoride-Releasing Restorative Materials: the Effect of a Resinous Coat on Ion Release

Katarina Kelić ; Stomatološka poliklinika Zagreb, Hrvatska
Matej Par orcid id orcid.org/0000-0002-2846-1840 ; Zavod za endodonciju i restaurativnu stomatologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Zagreb, Hrvatska
Kristina Peroš ; Katedra za farmakologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Zagreb, Hrvatska
Ivana Šutej ; Katedra za farmakologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Zagreb, Hrvatska
Zrinka Tarle ; Zavod za endodonciju i restaurativnu stomatologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Zagreb, Hrvatska


Puni tekst: engleski pdf 341 Kb

str. 371-381

preuzimanja: 1.153

citiraj

Puni tekst: hrvatski pdf 341 Kb

str. 371-381

preuzimanja: 204

citiraj


Sažetak

Objective: To determine the effect of two adhesive systems and a glass ionomer coating resin on fluoride release and concurrent pH changes over a period of 168 days. Material and methods: Four restorative materials were investigated: a giomer Beautiful II, an “alkasite” material Cention, a conventional composite Filtek Z250, and a glass ionomer cement Fuji IX Extra. Light-cured composite specimens were coated using G-aenial Bond and Clearfil Universal Bond Quick. Glass ionomer specimens were coated using GC Fuji Coat LC. Uncoated specimens were used as references. Quantitative fluoride release and pH changes were measured after 1 h, 24 h, 2 days, 7 days, 28 days, 84 days, and 168 days. Results: The cumulative fluoride release after 168 days increased for uncoated specimens in the following order: Filtek Z250 < Beautifil II < Cention < Fuji IX Extra. A comparatively lower fluoride release was measured for the composites coated with Clearfil Universal Bond Quick, with cumulative values after 168 days increasing in the following order: Filtek Z250 < Beautifil II < Cention. The composites coated with G-aenial Bond showed lower fluoride release compared to the uncoated specimens, with cumulative values increasing in the following order: Filtek Z250 < Beautifil II < Cention. The composites coated with G-aenial Bond showed pH values in the acidic range (4.4-5.7) after 1 h and 24 h. Conclusion: Fluoride release varied among the investigated restorative materials and depended on the use of dental adhesives and coatings. The pH of all materials, coating types and time points varied.

Ključne riječi

Dental Cements; Fluorides; Hydrogen-Ion Concentration; Drug Liberation