Skip to the main content

Original scientific paper

High-Temperature Investigation of the Properties of Blast Furnace Coke

A. Konstanciak


Full text: english pdf 97 Kb

page 235-237

downloads: 455

cite


Abstract

The behavior of coke in the blast furnace is discussed in this article. The methods of taking charge coke samples from blast furnace have been verified. The tests of the effect of temperature on coke (subjected to laboratory tests reproducing, to a certain extent, the conditions prevailing at the tuyere level of the blast furnace) have established factors responsible for the degradation of coke. This has allowed the parameters characterizing the structure to be described as follows: Lc, the crystallite height is contained in range 1.5932 - 3.2620 nm; La, the crystallite width is in the range 2.82013 - 5.7737 nm; and the crystallinity factor, Wk, is contained in the range 0.147 - 0.77014.

Keywords

Hrčak ID:

128396

URI

https://hrcak.srce.hr/128396

Publication date:

1.10.2003.

Article data in other languages: croatian

Visits: 1.355 *