Failures of dies for die-casting of aluminium alloys

B. Kosec


Full text: english pdf 1.077 Kb

page 51-55

downloads: 4.139

cite


Abstract

Die-casting dies for casting of aluminum alloys fail because of a great number of different and simultaneously operating factors. Material selection, die design, and thermal stress fatigue generated by the cyclic working process (heat checking), as well as to low and inhomogeneous initial die temperature contribute to the failures and cracks formation on/in dies for die-casting of aluminium alloys. In the frame of the presented investigation work the intensity and homogeneity of the temperature fields on the working surface of the testing die were checked through thermographic measurements, and failures and cracks on the working surface of the die were analysed with non-destructive metallographic examination methods.

Keywords

die-casting; working surface; aluminium alloy; temperature field; failure analysis

Hrčak ID:

17792

URI

https://hrcak.srce.hr/17792

Publication date:

1.1.2008.

Article data in other languages: croatian

Visits: 5.137 *