Topographic inspection as a method of weld joint diagnostic

Jolanta B. Krolczyk ; Opole University of Technology, 76 Proszkowska Street, 45-758 Opole, Poland
Bartosz Gapinski ; Faculty of Mechanical Engineering and Management, Poznan University of Technology, 3 Piotrowo Street, 60-965 Poznan, Poland
Grzegorz M. Krolczyk ; Opole University of Technology, 76 Proszkowska Street, 45-758 Opole, Poland
Ivan Samardzic ; Mechanical Engineering Faculty in Slavonski Brod, J. J. Strossmayer University of Osijek, Trg Ivane Brlić Mažuranić 2, 35 000 Slavonski Brod, Croatia
Radoslaw W. Maruda ; Faculty of Mechanical Engineering, University of Zielona Gora, 4 Prof. Z. Szafrana Street, 65-516 Zielona Gora, Poland
Kamil Soucek ; Institute of Geonics AS CR, v. v. i. Studentska 1768, Ostrava-Poruba, 708 00, Czech Republic
Stanislaw Legutko   ORCID icon orcid.org/0000-0001-8973-5035 ; Faculty of Mechanical Engineering and Management, Poznan University of Technology, 3 Piotrowo Street, 60-965 Poznan, Poland
Piotr Nieslony ; Opole University of Technology, 76 Proszkowska Street, 45-758 Opole, Poland
Yashar Javadi ; Department of Mechanical Engineering, Semnan Branch, Islamic Azad University, Semnan, Iran
Lubomir Stas ; Institute of Geonics AS CR, v. v. i. Studentska 1768, Ostrava-Poruba, 708 00, Czech Republic

Puni tekst: engleski, pdf (1 MB) str. 301-306 preuzimanja: 396* citiraj
APA
Krolczyk, J.B., Gapinski, B., Krolczyk, G.M., Samardzic, I., Maruda, R.W., Soucek, K., Legutko, S., Nieslony, P., Javadi, Y., Stas, L. (2016). Topographic inspection as a method of weld joint diagnostic. Tehnički vjesnik, 23(1). doi:10.17559/TV-20141230182054
Puni tekst: hrvatski, pdf (1 MB) str. 301-306 preuzimanja: 91* citiraj
APA
Krolczyk, J.B., Gapinski, B., Krolczyk, G.M., Samardzic, I., Maruda, R.W., Soucek, K., Legutko, S., Nieslony, P., Javadi, Y., Stas, L. (2016). Topografsko ispitivanje kao metoda za dijagnosticiranje stanja zavarenog spoja. Tehnički vjesnik, 23(1). doi:10.17559/TV-20141230182054

Sažetak
The paper demonstrates a topographic inspection in the specific context of three kinds of inspection methods of austenitic stainless steel welds. Visual and metrological inspection was analysed during tungsten inert gas (TIG) welding tests, showing the non-destructive techniques: X-ray, computed tomography, and surface profilometry. The article is a response to the lack of information, especially in the area of non-destructive techniques suitable for wide practical application. The Paper presents advantages and drawbacks of the analysed diagnostic methods and a classification of conventional and specific welded joint flaws. The most important defect in practical applications determining reliability of a welded joint is cracks. This kind of diagnostic is based on the obtained information about anisotropic and inhomogeneous volume under consideration in the heat-affected zone of a weld.

Ključne riječi
computed tomography; non-destructive techniques; profilometry; topography inspection; weld quality; X-ray