The structure of coatings and their ability to protect the castings made of G-X25NiCrSi 36-17 (DIN 17006) cast steel against carburization have been described. Al-Cu and Al-Si protective coatings, produced directly in a casting mould, have a considerable thickness (400 - 2000 µm), and complex multiphase structure. Its main structural constituents are: (Fe, Ni, Cr), (Fe, Ni, Cr), Al(Ni, Fe), carbides M23C6 and M7C3. In Al-Si ferritic coatings are also present: (Ni, Fe), (Fe, Al, Ni, Cr) and (Cr, Si)3Ni2Si. Carburisation changes substantially the structure of coatings, what results in an increase of the amount of (Fe, Ni, Cr) or (Ni, Fe) and carbides, and a decrease of the amount of (Fe, Ni, Cr) and Al(Ni, Fe). Apart from above mentioned changes, the investigated coatings reduce the carbon diffusion by 20 - 65 % Al-Cu, about 55 % Al-Si (austenitic), and 75 % Al-Si (ferritic), so they can provide a temporary protection against high-temperature corrosion.

Ključne riječi

Hrčak ID:

128394

URI

https://hrcak.srce.hr/128394

Datum izdavanja:

1.10.2003.

Podaci na drugim jezicima: hrvatski

Posjeta: 1.216 *