Assessment of Cytotoxic and Genotoxic Effect of Fissure Sealants in Buccal Epithelial Cells

Lidia Gavić ; Studij dentalne medicine pri Medicinskom fakultetu Sveučilišta u Splitu, Hrvatska
Kristina Goršeta ; Zavod za dječju i preventivnu stomatologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Hrvatska
Anita Buterin ; student Studija dentalne medicine pri Medicinskom fakultetu Sveučilišta u Splitu, Hrvatska
Domagoj Glavina ; Zavod za dječju i preventivnu stomatologiju Stomatološkog fakulteta Sveučilišta u Zagrebu, Hrvatska
Davor Želježić ; Institut za medicinska istraživanja i medicinu rada, Zagreb, Hrvatska
Antonija Tadin ; Studij dentalne medicine pri Medicinskom fakultetu Sveučilišta u Splitu, Hrvatska


Puni tekst: engleski pdf 341 Kb

str. 10-17

preuzimanja: 506

citiraj

Puni tekst: hrvatski pdf 341 Kb

str. 10-17

preuzimanja: 169

citiraj


Sažetak

Aim: The main purpose of this study was to assess the genotoxic and cytotoxic effect of fissure sealants on buccal epithelial cells. Material and methods: The study was conducted on 45 patients (27 girls and 18 boys), seven to 16 years of age (age mean 12.09 ± 2.20). Buccal swabs were collected before (T0), seven (T1), 30 (T2) and 90 days (T3) consequently after fissure sealant placement (Heli-oseal F®, Equia Fil®, Constic®). Patients or legal guardians filled in the questionnaire regarding the demographic data (age, gender), dietary habits, health status, medication usage, and recent X-ray exposure. DNA damage was analyzed using the micronucleus test. Results: Statistically significant difference in the number of buccal cells with condensed chromatin was found between T0 (time before fissure sealant placement) and T3 (90 days after fissure sealant placement) period for Helioseal F® (P = 0.025). For the other two analyzed materials, no difference was observed during the tested period. There was no difference between materials in the same sampling time. Conclusion: Apart from an increase in cells with condensed chromatin 90 days after the placement of Helioseal F®, no other nuclear abnormalities were observed for tested fissure sealants. Although these sealants have now largely been used, it is of high importance that their biocompatibility is checked continuously, especially in in vivo clinical studies

Ključne riječi

MeSH terms: Pit and Fissure Sealants; Materials Testing; Mutagenicity Tests; Cytotoxins; Epithelial Cells. Author keywords: Biocompatibility; Buccal epithelial cells; Fissure seal-ants; Micronucleus assay