Abstract

In this paper the influence of cooling time in temperature interval from 800 to 500 °C (Δt8/5) on hardness and impact strength of thermal cycle simulated specimens from high strength fine grained steel TStE 420 is explained. Also a research on scanning electron microscope and fractography analysis of characteristic fractures on simulated specimens is performed.