Abstract
The investigation concerned the use of sinter containing a titanium-vanadium-magnetite concentrate for the production of pig iron. Sinter containing 0,46 to 0,51 % TiO2 and 0,056 to 0,060 % vanadium was used for pig iron production in the blast furnace. Introducing 200 kg of this concentrate to the1 Mg sinter mix did not cause any deterioration of sinter quality.
Keywords
blast furnace; sinter; titanium-vanadium-magnetite concentrate