Heat treatment influence on clad dissimilar joints weakness

Branko Mateša ; Mechanical Engineering Faculty in Slavonski Brod, J. J. Strossmayer University of Osijek, Trg Ivane Brlić Mažuranić 2, 35 000 Slavonski Brod, Croatia
Ivan Samardžić ; Mechanical Engineering Faculty in Slavonski Brod, J. J. Strossmayer University of Osijek, Trg Ivane Brlić Mažuranić 2, 35 000 Slavonski Brod, Croatia
Marko Dunđer ; Faculty of Philosophy, University of Rijeka, Department of Polytechnic, Omladinska 14, 51 000 Rijeka, Croatia


Full text: croatian pdf 1.150 Kb

page 1035-1040

downloads: 995

cite

Full text: english pdf 1.150 Kb

page 1035-1040

downloads: 502

cite


Abstract

The dissimilar specimens (ASTM A387 Gr.12 + ASTM A240 TP 304L) clad by different procedures (explosion welding, submerged arc welding–surfacing using strip electrode (SAW) and hot rolling) were heat treated (650 °C through 2 hours). The shear strength testing of clad joints and Charpy impact energy testing were performed. The statistical analysis of testing results was elaborated, and the significance of heat treatment influences on the clad joints weakness was established.

Keywords

clad joints; heat treatment; shear strength