Otpuštanje fluora iz staklenog ionomera tretiranog s dva različita premaza

Valentina Brzović Rajić ; Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Croatia
Ivana Miletić ; Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Croatia
Sevil Gurgan ; School of Dental Medicine, Hacettepe University, Ankara, Turkey
Kristina Peroš ; Department of Pharmacology, School of Dental Medicine, University of Zagreb, Croatia
Željko Verzak ; Department of Pediatric and Preventive Dentistry, School of Dental Medicine, University of Zagreb, Croatia
Ana Ivanišević Malčić ; Department of Endodontics and Restorative Dentistry, School of Dental Medicine, University of Zagreb, Croatia


Full text: croatian pdf 443 Kb

page 307-313

downloads: 352

cite

Full text: english pdf 443 Kb

page 307-313

downloads: 1.235

cite


Abstract

Svrha rada: Ovo istraživanje in vitro uspoređuje otpuštanje fluora iz mikrolaminiranog staklenog ionomera temeljenog na stakleno-hibridnoj tehnologiji premazanog dvama različitim premazima. Materijali i postupci: Ukupno 18 uzoraka podijeljeno je u skupine po šest uzoraka: (1) stakleni ionomer Equia Forte Fil premazan Equia Forte Coatom (Equia + EC), (2) stakleni ionomer Equia Forte Fil premazan GC Fuji Varnishem (Equia + VC) i (3) nepremazani stakleni ionomer Equia Forte (EQUIA kont). Otpuštanje fluora mjereno je fluor-selektivnom elektrodom (ORION EA 940) nakon 24 sata, 4 dana, 30 dana i 64 dana. ANOVA, Tukeyjev test multiplih usporedbi i paired t-test korišteni su u testiranju razlika među skupinama. Rezultati: Statistički značajne bile su razlike među skupinama i četirima točkama u vremenu (ANOVA, p < 0,0001). Kumulativno otpuštanje iona fluora nakon 64 dana bilo je redom 66,01 mg/l, 123,54 mg/l i 203,22 mg/l za EQUIA + EC, EQUIA + VC i EQUIA kont. Sve su razlike bile statistički značajno različite, osim one između EQUIA + VC i EQUIA kont. nakon 24 sata. Zaključci: Količina otpuštenog fluora bila je značajno manja u uzorcima premazanima nanopunjenim premazom u usporedbi s onima premazanima varnishem i bez premaza.

Keywords

stomatološki materijali; fluoridi; staklenoionomerni cementi; nanočestice; lak