Skip to the main content

Preliminary communication

Defects analysis of copper wires manufactured in industrial conditions

M. Zasadzinska orcid id orcid.org/0000-0002-3455-3469 ; AGH University of Science and Technology, Faculty of Non-Ferrous Metals, Cracow, Poland
B. Smyrak ; AGH University of Science and Technology, Faculty of Non-Ferrous Metals, Cracow, Poland
T. Knych ; AGH University of Science and Technology, Faculty of Non-Ferrous Metals, Cracow, Poland
P. Strzepek orcid id orcid.org/0000-0002-5495-1253 ; AGH University of Science and Technology, Faculty of Non-Ferrous Metals, Cracow, Poland


Full text: english pdf 492 Kb

page 774-776

downloads: 1.767

cite


Abstract

Many factors are responsible for the formation of surface and internal defects during copper wire drawing process. Generally they may be divided into defects of material or processing origin. Even input material of the highest quality with little to none defects cannot ensure the absence of breakages during the process due to inadequate process parameters. Optimally selected process parameters may reduce the risk of cracks forming during the metal forming process. The paper presents examples of wire defects and cracks occurring throughout the wire drawing process of copper in industrial conditions and a wide analysis of their source.

Keywords

copper wires; drawing process; wire defects; fracture; scanning electron microscopy (SEM)

Hrčak ID:

274036

URI

https://hrcak.srce.hr/274036

Publication date:

1.7.2022.

Visits: 2.295 *