Measurements of the dielectric properties of liquid selenium and Se-Tl-S alloys were carried out at different frequencies and temperatures. It was found that the frequency at the maximum dielectric loss shifts towards high frequencies and increasing temperature. The dielectric relaxation activation energy was calculated and correlated with the electrical conduction activation energy.