hrcak mascot   Srce   HID

Prethodno priopćenje

Corrosion of the WE43 and MSR-B magnesium alloys in CO2

R. Przeliorz ; The Silesian University of Technology, Katowice, Poland
J. Piątkowski ; The Silesian University of Technology, Katowice, Poland

Puni tekst: engleski, pdf (331 KB) str. 429-432 preuzimanja: 268* citiraj
APA 6th Edition
Przeliorz, R. i Piątkowski, J. (2016). Corrosion of the WE43 and MSR-B magnesium alloys in CO2. Metalurgija, 55 (3), 429-432. Preuzeto s https://hrcak.srce.hr/153639
MLA 8th Edition
Przeliorz, R. i J. Piątkowski. "Corrosion of the WE43 and MSR-B magnesium alloys in CO2." Metalurgija, vol. 55, br. 3, 2016, str. 429-432. https://hrcak.srce.hr/153639. Citirano 19.07.2019.
Chicago 17th Edition
Przeliorz, R. i J. Piątkowski. "Corrosion of the WE43 and MSR-B magnesium alloys in CO2." Metalurgija 55, br. 3 (2016): 429-432. https://hrcak.srce.hr/153639
Harvard
Przeliorz, R., i Piątkowski, J. (2016). 'Corrosion of the WE43 and MSR-B magnesium alloys in CO2', Metalurgija, 55(3), str. 429-432. Preuzeto s: https://hrcak.srce.hr/153639 (Datum pristupa: 19.07.2019.)
Vancouver
Przeliorz R, Piątkowski J. Corrosion of the WE43 and MSR-B magnesium alloys in CO2. Metalurgija [Internet]. 2016 [pristupljeno 19.07.2019.];55(3):429-432. Dostupno na: https://hrcak.srce.hr/153639
IEEE
R. Przeliorz i J. Piątkowski, "Corrosion of the WE43 and MSR-B magnesium alloys in CO2", Metalurgija, vol.55, br. 3, str. 429-432, 2016. [Online]. Dostupno na: https://hrcak.srce.hr/153639. [Citirano: 19.07.2019.]

Sažetak
The kinetics of WE43 and MSR-B magnesium alloys oxidation was tested in CO2 atmosphere. The measurement of the oxidation speed was conducted with continuous thermo gravimetric method in the eutectic melting temperature (530 °C). This temperature has been defined with the differential scanning calorimetric (DSC) method. The corrosion products were analyzed with Scanning Electron Microscopy (SEM) and Energy Disspersive X-ray Spectroscopy (EDS) methods. On the WE43 alloy the double layer scale is being created, with good protective properties. Under the scale layer the internal oxidation of the alloy takes place. The oxide layer on MSR-B alloy is thin and irregular.

Ključne riječi
corrosion; cast magnesium alloys; oxidation; structure; CO2 atmosphere