Surface Charging of Zinc Oxide During XPS Examination
M. Mintas
; Institut fur Radiochemie, Kernforschungszentrum Karlsruhe, 7500 Karlsruhe, Postfach 3640, Germany
W. G. Filby
; Institut fur Radiochemie, Kernforschungszentrum Karlsruhe, 7500 Karlsruhe, Postfach 3640, Germany
Sažetak
Surface charging of zinc oxide during XPS examination has
been studied. The magnitude of the charge is 0.4-0.6 eV at room
temperature and decreases at higher temperature to almost zero
(nominal 0.1 eV at 300 °C) . Reproducible BE values can only be
achieved after correction for this charging. Possible mechanisms are
briefly discussed.