Development and optimisation of curing temperature of energy-efficient geopolymer bricks

Rupali B. Kejkar
Swapnil P. Wanjari


Puni tekst: engleski pdf 335 Kb

str. 411-420

preuzimanja: 414

citiraj

Puni tekst: hrvatski pdf 333 Kb

str. 411-420

preuzimanja: 307

citiraj


Sažetak

Present study focuses on development of a sustainable geopolymer brick in which the use of fly ash is maximised and the concentration of an alkaline solution without cement is reduced, in order to reduce environmental burden and carbon emissions. The geopolymer bricks were developed using the Class F fly ash with 2 to 4 Molar alkaline solution. The bricks were cured for one hour at temperatures ranging from 100 to 600°C. The compressive strength of such bricks amounts to 10.2 MPa and was achieved in the 4-Molar alkaline solution at the curing temperature of 400°C. The geopolymer bricks exhibit crystalline structure and good thermal insulation properties.

Ključne riječi

geopolymer brick; fly ash; alkaline solution; curing temperature; physicomechanical properties