hrcak mascot   Srce   HID

Preliminary communication

The corrosion resistant coating with halloysite nanoparticles

A. Z. Issagulov ; Karaganda State Technical University, Karaganda, Kazakhstan
V. Yu. Kulikov ; Karaganda State Technical University, Karaganda, Kazakhstan
Y. P. Chsherbakova ; Karaganda State Technical University, Karaganda, Kazakhstan
T. V. Kovaleva ; Karaganda State Technical University, Karaganda, Kazakhstan
Sv. S. Kvon ; Karaganda State Technical University, Karaganda, Kazakhstan

Fulltext: english, pdf (261 KB) pages 426-428 downloads: 229* cite
APA 6th Edition
Issagulov, A.Z., Kulikov, V.Y., Chsherbakova, Y.P., Kovaleva, T.V. & Kvon, S.S. (2016). The corrosion resistant coating with halloysite nanoparticles. Metalurgija, 55 (3), 426-428. Retrieved from https://hrcak.srce.hr/153638
MLA 8th Edition
Issagulov, A. Z., et al. "The corrosion resistant coating with halloysite nanoparticles." Metalurgija, vol. 55, no. 3, 2016, pp. 426-428. https://hrcak.srce.hr/153638. Accessed 25 Jan. 2020.
Chicago 17th Edition
Issagulov, A. Z., V. Yu. Kulikov, Y. P. Chsherbakova, T. V. Kovaleva and Sv. S. Kvon. "The corrosion resistant coating with halloysite nanoparticles." Metalurgija 55, no. 3 (2016): 426-428. https://hrcak.srce.hr/153638
Harvard
Issagulov, A.Z., et al. (2016). 'The corrosion resistant coating with halloysite nanoparticles', Metalurgija, 55(3), pp. 426-428. Available at: https://hrcak.srce.hr/153638 (Accessed 25 January 2020)
Vancouver
Issagulov AZ, Kulikov VY, Chsherbakova YP, Kovaleva TV, Kvon SS. The corrosion resistant coating with halloysite nanoparticles. Metalurgija [Internet]. 2016 [cited 2020 January 25];55(3):426-428. Available from: https://hrcak.srce.hr/153638
IEEE
A.Z. Issagulov, V.Y. Kulikov, Y.P. Chsherbakova, T.V. Kovaleva and S.S. Kvon, "The corrosion resistant coating with halloysite nanoparticles", Metalurgija, vol.55, no. 3, pp. 426-428, 2016. [Online]. Available: https://hrcak.srce.hr/153638. [Accessed: 25 January 2020]

Abstracts
The process of application of coating on metal surfaces is described in this article. The composition with 100 % corrosion preventing substance + 42,5 % acetone + 10 % halloysite was recognized as the most appropriate for coating, and it provides the best corrosion resistance of hydraulic pump details. The impellers of circulation pumps for water delivery in heating system fail after 5 - 6 months because of the galling of work flutes, as water doesn’t pass through the chemical purification. After applying corrosion resistant coating with halloysite the lifetime of impellers increases. The essence of which is dipping the impeller into hydrochloric acid with 24 hour keeping in it, then it is dried in dryer up to 4 hours. The lifetime of this impeller increases 1,8 fold and it was approximately 9 months.

Keywords
corrosion; surface; coating; polystyrene foam; quality